Share your drawing, material requirements, annual volume, tolerance needs, or application details. Our engineering team will review your MIM project and respond with technical feedback or a quotation.
Fe-2Ni (MIM-2200) is a low alloy steel used in metal injection molding (MIM) for small, complex precision components. Explore its mechanical properties, heat treatment options, and suitability for structural and moving parts. Compare Fe-2Ni with other MIM low alloy steels based on strength, hardness, wear resistance, and dimensional requirements. XTMIM supports material selection, DFM, manufacturing feasibility review, and sample validation before tooling.
Low Alloy Steel MIM Parts & Image Reference Catalogue
Explore low-alloy steel MIM part references by material grade, starting with 4605. Material-verified examples are identified separately from unconfirmed part photos and illustrations. A workbook category is not proof that the individual pictured part uses that grade.
Source status: 9 records have documented grade descriptions (including two with separate image-use restrictions); 6 image references lack part-specific grade or photograph matching. These examples come from third-party publications, not XTMIM production projects. Image reproduction rights require confirmation.
4605 Archive
7 entries · 5 documented MIM-4605 parts and 2 unmatched image references
U-shaped clamp body with bosses and pin features. Published as an MIM-4605 part; the source discusses filling, cooling and venting around unequal sections.
Photograph shows a central opening, radial ribs and surrounding holes. A separate MIM-4605 shock-absorber plate case exists, but this photo has not been matched to that part.
Small three-legged valve component for diesel fuel injection. The published case highlights outside diameter, leg perpendicularity and sintering support.
Ring-shaped component with exterior teeth and internal engagement details. The related page describes an MIM-8620 pinion ring, but its figure caption differs; this photo-to-part mapping is unresolved.
Published right- and left-hand threaded inserts used in a folding-roof clamp and hinge mechanism. Original photograph contains an unrelated third-party brand marking.
Three-piece quick-disconnect fitting. The original source also documents a restricted end use; retained only for internal material research, not public site use.
Splined ratchet shaft for an electronic parking-brake mechanism. The cited source identifies AISI 4140-equivalent steel and special sintering fixtures to control geometry.
Several shafts, a split clamp, brackets and small connectors on a blue background. Individual alloy, manufacturing route and end-use are not established by the available photo record.
Rendered image of toothed gripper jaws. Zimmer Group has discussed MIM gripper applications, but this artwork does not prove the displayed parts are MIM 4340.
Source: Zimmer / PIM International reference · Archive 28
Split cylindrical clamp and flat mounting plate with holes. Shown in a 4340-related supplier promotion; the pictured part’s alloy, process and application are not verified.
Flanged part with an internal spline, mounting holes and raised stepped post. A 4340-themed marketing image does not independently confirm the specific pictured part’s material.
Fe-2Ni (MIM-2200) is a low-carbon, nickel-alloyed steel used in metal injection molding (MIM). It is a candidate for compact mechanical parts when the specified material condition can meet the required strength, ductility and service conditions. The alloy is not corrosion-resistant stainless steel, nor a direct substitute for heat-treated 4605, 4140 or 4340. The drawing, contact surfaces and final processing route determine whether it is suitable.
Fe-2Ni selection at a glance
Fe-2Ni / MIM-2200 is worth considering for small, complex parts whose loads and assembly functions can be met by a specified low-carbon Fe-Ni material. First establish the actual grade: Fe2Ni and Fe02Ni are common shorthand forms, FN02 is a supplier designation associated with MIM-2200, and FN0205 is a different, higher-carbon grade. Where strength, fatigue life, wear or corrosion requirements cannot be met by the proposed material and treatment, compare other grades. Before tooling, define the final material state, critical dimensions and acceptance tests.
ConsiderSmall MIM-suitable geometry, defined static loads and a verifiable low-carbon Fe-Ni specification.
VerifyMoving contacts, dimensional stability after treatment, case requirements and fatigue-sensitive duty cycles.
Compare alternativesHigh bulk strength, severe corrosion, demanding wear life or another specified alloy family.
Published Fe-2Ni applications include an Fe-2% Ni manual-transmission shift lever reported by GKN / PIM International and Fe2Ni cage and plate components in a Schunk robot gear assembly. Both are third-party manufacturing examples; their published descriptions do not establish an ASTM MIM-2200 certification or an XTMIM production record.
01 · Confirm the material
What Is Fe-2Ni (MIM-2200), and How Is It Specified?
Fe-2Ni denotes an iron-based alloy with approximately 2% nickel. In MIM specifications, the relevant low-carbon grade is commonly identified as MIM-2200. ASTM B883-24 lists MIM-2200 as a ferrous MIM low-alloy-steel designation; it also lists MIM-4605 and MIM-4140 separately. The purchasing drawing should identify the applicable grade and standard edition, rather than rely on the term Fe-2Ni alone. ASTM B883-24 overview.
Chemical Composition and MIM-2200 Material Designation
Published Fe-2Ni / MIM-2200 data sheets show the following chemistry limits. These values help check a drawing or supplier quotation; final acceptance must follow the agreed material specification and edition.
Element
Published reference (wt%)
Source and engineering use
Nickel (Ni)
1.5–2.5%
PolyMIM FN02, Parmaco Fe2Ni and APP MIM 2200 references; confirm on drawing and material order.
Carbon (C)
≤ 0.10%
Low-carbon FN02 / MIM-2200 reference. Do not interchange with higher-carbon FN0205.
Molybdenum (Mo)
≤ 0.50%
Parmaco / APP reference ceiling; check the approved material sheet rather than assuming an intentional Mo addition.
Silicon (Si)
≤ 1.0%
APP's MIM-2200 composition listing; confirm any customer-specific limits.
FN02, FN0205 and MIM-2200 must not be approved as interchangeable names. For example, PolyMIM lists FN02 / MIM 2200 with carbon at 0.1% maximum, while its FN0205 feedstock has 0.4–0.6% carbon. The higher carbon content changes the material's potential hardening response and mechanical-property range. Heat-treated values for FN0205 must not be assigned to low-carbon FN02.
Designation encountered
How to interpret it
Required confirmation
MIM-2200
Recognized low-alloy-steel MIM designation
Applicable standard edition, chemistry, condition and acceptance values.
Fe-2Ni / Fe2Ni / Fe02Ni
Common alloy descriptions or shorthand
Whether the intended grade is low-carbon MIM-2200 / FN02.
FN02
Supplier designation used for low-carbon Fe-2Ni
Approved feedstock specification and finished-part condition.
FN0205
Higher-carbon Fe-Ni material in PolyMIM's portfolio
Separate grade approval; do not substitute its property values for FN02.
Specify the finished-part condition. Feedstock codes help source material, but the released drawing also needs the approved material standard or data sheet, final carbon requirement where applicable, heat treatment, target properties and acceptance method.
Unclear material callout: “2% Ni steel” alone does not define carbon, strength, hardness or final treatment. Resolve the grade and acceptance requirements before mold design. For the broader family, see MIM low alloy steel materials.
02 · Establish the performance basis
What Mechanical Properties Can Fe-2Ni MIM Steel Achieve?
Fe-2Ni properties depend on the feedstock, sintering process and finished material condition. Density, yield strength, tensile strength, elongation and hardness are useful selection inputs, provided the source and test condition are known. The part's load path, weakest section and post-processing determine how those numbers apply to the finished component.
As-Sintered Density, Strength, Ductility and Hardness
PolyMIM gives threshold values for its sintered FN02, while Parmaco reports ranges and minimums for as-sintered Fe2Ni. APP lists typical MIM 2200 values without naming the condition in the referenced table. These three data sets are shown separately because they are not interchangeable acceptance limits or XTMIM production guarantees.
APP also lists a Young's modulus of 190 GPa and unnotched Charpy impact energy of 135 J for its MIM 2200 entry. Neither value proves the impact resistance or fatigue life of a thin, notched or otherwise geometry-sensitive finished part. For a load-bearing part, a minimum allowable value, density requirement where relevant, sample location and test method should be agreed before releasing the drawing.
Using property data: Yield strength helps assess permanent deformation; ultimate tensile strength concerns fracture under tension; elongation describes ductility in the reported test condition. Hardness cannot replace a wear or fatigue test. A standard tensile specimen also does not capture every stress concentration or thin section in a molded part.
Heat Treatment, Surface Hardness and Final Material Condition
Low-carbon Fe-2Ni may be evaluated for case hardening when its service function depends on surface contact. APP lists a case-hardened reference hardness of 56–62 HRC for MIM 2200; Parmaco reports a maximum of 750 HV (approximately 62 HRC) and an effective hardened depth (EHT) of 0.05–0.5 mm in its historical Fe2Ni specification. These results are not universal Fe-2Ni properties: surface hardness and effective case depth must be qualified for the actual part.
Surface hardness, case depth and core properties answer different questions. A small latch tip may need a wear-resistant surface without requiring the entire section to reach the same hardness. A structural lever may instead be limited by section strength or deflection. The treatment route must be evaluated together with dimensional movement, contact geometry and the required inspection method.
After case hardening: Grinding, machining or polishing may remove part of the hardened layer. Measure hardness at the specified location and verify the remaining effective case depth. Core strength, dimensional stability and contact wear still require their own acceptance criteria.
FN0205 is a different grade: Its published heat-treated values cannot be used as FN02 / MIM-2200 properties. Specify the treatment, hardness scale, measurement location and required case depth for the actual material.
03 · Apply the data to the real part
Which Parts and Service Conditions Are Suitable for Fe-2Ni MIM?
A bracket may only locate an assembly, or it may carry the main structural load. Similarly, a hinge may move a few times or operate for thousands of cycles. The decision to use Fe-2Ni depends on the actual loads, mating surfaces, service environment and approved material condition—not on the part name.
Structural and Precision Assembly Components
Compact brackets, levers, links, latches, inserts and hinge components are potential Fe-2Ni applications where MIM can form repeated complex features. Their suitability depends on service conditions, and their production economics depend on tooling cost and volume. For structural parts, determine applied forces and load direction, minimum section, stiffness or allowable deformation, stress concentrations and assembly-fit dimensions. Check whether a local contact edge, thin web or small pin interface is more critical than the part's overall size.
Precision inserts and assembly features may be limited by hole position, perpendicularity, mating-face flatness, press-fit retention or post-treatment growth rather than bulk strength. In that case, inspect the final treated geometry against the assembly datum, rather than approving the grade from tensile values alone.
Moving and Contact Components: Wear and Surface Requirements
Wear depends on contact pressure, the mating material, surface roughness, lubrication, contamination and repeated movement. Fe-2Ni surface hardness alone cannot predict the service life of a moving joint. For sliding locks or small articulated parts, define mating materials, contact load, travel, lubrication and the permitted change in clearance or operating force over the planned cycle test. These conditions are needed before selecting between as-sintered Fe-2Ni, case-hardened Fe-2Ni or another alloy. Parmaco reports an as-sintered surface-roughness reference of Ra ≤ 1.6 µm for its own Fe2Ni material, but that value does not establish wear life or the finish of an unrelated production part.
Part or service requirement
Initial Fe-2Ni assessment
Evidence needed for the decision
Small bracket / housing insert
Reasonable candidate if load and fit are defined
Section stress or force requirement, mounting datums, critical dimensions and any corrosion exposure.
Lever / link / latch
Conditional
Load direction, permanent-deformation limit, impact or fatigue duty, bearing/contact geometry.
Hinge-related part / sliding contact
Conditional; surface treatment may be relevant
Surface-hardness and wear target, counterpart material, lubrication, cycle test and post-treatment fit.
Precision assembly feature
Possible with process-capability review
Tolerances after final processing, measurement datum and retention or mating fit.
Wet, salt-laden or aggressive chemical environment
Not a default choice
Corrosion requirement and comparison with stainless steel or protective solutions.
Safety-critical or fatigue-limited component
Do not select from a datasheet alone
Defined design loads, representative specimens, production traceability and duty-specific validation.
Published Fe-2Ni parts in automotive and robotics assemblies
The two published examples identify the Fe-Ni material and the components made from it. Their assembly functions suggest specific design checks, although the full load limits, tolerances and inspection results are not included in the source articles.
GKN Sinter Metals · passenger-car transmission shift lever · Fe-2% Ni.
Manual transmission shift lever — GKN Sinter Metals
Part and process: GKN made this passenger-car shift-lever component by MIM using Fe-2% Ni. The published sequence shows molding, sintering, case hardening and shaft assembly.
Critical checks: For a similar lever, define contact hardness, dimensions after hardening and shaft-assembly fit. The article does not specify numerical targets or the exact ASTM material designation.
Part and material: The five-piece MIM assembly contains three hardened 100Cr6 gears, an Fe2Ni cage and an Fe2Ni plate. Fe2Ni is used for the cage and plate, not the gear teeth.
Critical checks: Cage and plate positioning, alignment and loads should be specified separately from gear-tooth hardness and wear. The published article does not provide numerical service limits for those components.
Scope of the case evidence: Both publications identify Fe-2% Ni / Fe2Ni components, but neither reports the complete MIM-2200 chemistry, mechanical acceptance limits or dimensional tolerances. The examples are third-party cases, not XTMIM production records. A new part still needs its own material specification and qualification.
Wear-life specification: Initial assembly fit cannot establish long-term performance. For moving latches or levers, define the contact load, mating material, lubrication, operating cycles and maximum allowable clearance change before approving the material and treatment.
For corrosion-led designs, review MIM 316L stainless steel. For the wider range of actual part families and manufacturing approaches, see MIM low alloy steel parts. Other part types in the suitability table are engineering candidates, not documented XTMIM Fe-2Ni production programs.
04 · Decide whether to change grade
When Should You Consider Another MIM Steel Instead of Fe-2Ni?
Compare alloys against the loads, material condition, corrosion exposure, wear requirements and allowable processing cost for the specific part. Higher tensile strength is not always useful if the alternative needs a treatment that distorts critical dimensions or reduces the ductility required by the assembly.
Fe-2Ni vs Fe-4Ni and Fe-8Ni
Nickel content alone cannot determine the best Fe-Ni grade. Carbon, other alloying elements, sintered density and treatment condition also affect the final properties. For a higher-Ni family example, PolyMIM's sintered FN08 / MIM 2700 lists Ni at 6.5–8.5%, yield strength above 210 MPa and elongation above 20% under its stated conditions; this is a supplier-specific grade, not a universal Fe-8Ni design guarantee.
If the drawing nominates Fe-4Ni or Fe-8Ni, compare the exact material sheets and approved condition rather than estimating performance from the nominal nickel percentage alone.
Fe-2Ni vs MIM-4605, 4140 and 4340
Consider 4605, 4140 or 4340 when the specified strength, hardness or toughness cannot be met by the selected Fe-2Ni condition. Many high-strength values reported for these alloys refer to heat-treated material. Such figures cannot be compared directly with as-sintered Fe-2Ni data.
Material route
Why an engineer may investigate it
Condition that must be verified
Fe-2Ni / MIM-2200
Low-carbon Fe-Ni candidate with published ductility and potential surface-hardening route
Load requirement, exact grade, final surface and dimensional condition.
Supplier-specific treated properties, ductility, dimensional effect and fatigue evidence.
The table identifies when each grade warrants investigation; it does not rank mechanical properties under a single test condition. The linked material pages provide grade-specific details. See also MIM material selection guidance.
PolyMIM sintered-state properties: Fe-2Ni and alternative grades
PolyMIM publishes these sintered-state threshold values for several feedstock grades. Using one supplier's data reduces variation in data reporting, but it does not eliminate differences in alloy chemistry or prove that one grade is best for a particular part. These values are not ASTM minimums or XTMIM production specifications.
PolyMIM grade (sintered)
0.2% yield
Tensile strength
Elongation
Selection context
FN02 / MIM-2200
> 150 MPa
> 260 MPa
> 20%
Low-carbon Fe-2Ni baseline
FN08 / MIM-2700
> 210 MPa
> 380 MPa
> 20%
Higher-nickel Fe-Ni route; not a validated substitute for every Fe-8Ni drawing
MIM-4605
> 400 MPa
> 600 MPa
> 5%
Carbon / molybdenum-containing alloy; treatment can change final results
MIM-4140
> 400 MPa
> 700 MPa
> 3%
Cr-Mo route; confirm specification and final condition
MIM-4340
> 500 MPa
> 700 MPa
> 11%
Ni-Cr-Mo route; qualify intended treatment and performance
Source: PolyMIM feedstock portfolio, Low Alloys table (page 1). All figures shown are published threshold values for the named supplier's sintered condition; they are not a universal material ranking. No equivalent Fe-4Ni data are presented in this source, so no numeric Fe-4Ni comparison is inferred. Do not compare these values directly with APP's heat-treated 4605, 4140 or 4340 table.
MIM-4605 clamp body · INDO-MIM / MPIF Design Excellence Awards.
Published MIM-4605 component
Component and process: MPIF identifies INDO-MIM's hand-power-tool clamp body as MIM-4605. The U-shaped part has bosses and pin-like projections; the manufacturing account describes cooling and venting controls used to limit voids and weld lines.
Selection relevance: This is a documented MIM-4605 manufacturing example, not a Fe-2Ni strength comparison. A substitute grade must still meet the drawing's final-state properties and manufacturing requirements.
What Determines Fe-2Ni MIM Manufacturing Feasibility?
Suitable alloy chemistry does not guarantee a manufacturable MIM part. Feedstock qualification, geometry-dependent shrinkage and post-processing can determine whether the finished component meets tolerance and mechanical requirements. These issues belong in the material and DFM review before the mold is released.
Feedstock Availability and Sintered Material Control
Confirm that a viable Fe-2Ni / MIM-2200 feedstock and sintering route can be supported by the selected producer. Published feedstock data are a useful starting point, but part density, residual carbon, dimensional repeatability and mechanical properties depend on the specific powder, binder, debinding route, furnace atmosphere and process window.
PolyMIM reports a 1.2160 shrinkage factor for a specified FN02 feedstock configuration. It is a feedstock-dependent tooling reference, not a universal shrinkage percentage or a validated mold-scaling formula. The tooling allowance must be established for the actual feedstock, geometry and sintering route.
Shrinkage, Critical Dimensions and Secondary Operations
The critical manufacturing review starts with functional surfaces and datums. Uneven wall thickness, slender projections, gate position, sintering support and long unsupported spans may create filling, handling or distortion problems. A subsequent case-hardening or other thermal process can affect fit, straightness or hole size, requiring final inspection or machining allowances.
Manufacturing risk
Likely consequence
Practical control before tooling
Feedstock and grade not qualified
Uncertain chemistry, density or material response
Confirm feedstock source, target specification and trial/acceptance route.
Thin-to-thick transitions
Nonuniform shrinkage and geometric drift
Review transitions, wall distribution and sintering support.
Delicate green features or thick enclosed regions
Handling damage or debinding defects
Review ejection support, debinding pathway and sample-inspection checkpoints.
Gate on a functional surface
Surface discontinuity or added finishing work
Move or review gate location during DFM.
Tight holes, mating faces or datums
Assembly fit outside post-sintering capability
Plan final-process tolerance and possible sizing or machining.
Hardening after sintering
Dimension changes or loss of flatness
Define inspection after treatment, case requirements and rework route if needed.
Limited annual volume
Tooling cost cannot be economically amortized
Compare total MIM tooling/sample costs with CNC or other processes at the forecast volume.
Critical-feature plan: Record each functional dimension in its required final state—as-sintered, sized, machined or case-hardened. A lever's mating bore and contact surface may need inspection after heat treatment; a robot cage or plate may be governed by position and flatness. Neither requirement can be guaranteed from a generic shrinkage factor.
For detailed geometry and tolerance decisions, use the MIM DFM guide and MIM tolerance strategy. For the effect of post-sintering operations on hard-to-hold dimensions, review post-sintering machining. For Fe-2Ni, prioritize the risks that affect the actual part's critical features and final material condition.
06 · Specify, inspect and qualify
How Should an Fe-2Ni MIM Project Be Specified and Validated?
An Fe-2Ni project needs an agreed material specification, finished-part drawing and test criteria. The RFQ establishes those requirements; acceptance criteria should be settled before tooling, and initial samples must show that the part and production route meet them.
What to Include in an Fe-2Ni MIM Drawing and RFQ
Drawing and design information
2D drawing and 3D CAD geometry
Critical dimensions, datums and tolerances
Assembly interfaces and functional surfaces
Expected annual volume and batch size
Material and service information
Exact Fe-2Ni / MIM-2200 callout and allowed alternatives
Required strength, ductility, density or hardness
Heat treatment / surface condition
Load, contact, corrosion or cycle requirements
Where a numerical requirement has not been set, provide the part function, load and failure concern. The supplier can then recommend a testable target for approval instead of copying an unrelated data-sheet value into the drawing.
Define Material and Part Acceptance Criteria Before Tooling
ASTM B883 is a ferrous MIM material specification, while MPIF Standard 35-MIM is a material-selection and specification resource. The MPIF notes that purchaser and manufacturer should agree on grade, chemistry, strength, proof testing and application-relevant processes before production. MIMA identifies the 2025 edition as the current Standard 35-MIM edition.
Requirement to approve
Useful evidence
Decision it supports
Grade and composition
Approved material specification, feedstock traceability or agreed chemistry test
Correct low-carbon Fe-2Ni material, not a similar name.
Density / mechanical properties
Defined test specimens, test method and measured results in stated condition
Measured values meet the contractual criteria.
Case hardening or final hardness
Final-state hardness report, location, scale and case-depth measure where applicable
Functional contact requirement and local material condition are met.
Critical dimensions and surfaces
Final-process dimensional inspection, datum method, roughness or surface review
Assembly fit after sintering and any thermal treatment.
Wear, fatigue, impact or cyclic function
Application-specific functional test and acceptance threshold
The real part works under the stated service condition.
Material certificates and tensile coupons characterize the tested material. They cannot establish the service life of a notched section, press-fit insert or sliding interface. Add a part-level acceptance test where geometry or contact conditions create a different failure mode.
Sample Qualification and Production Approval
Before tooling: confirm grade, final condition, key functional dimensions, inspection methods and the feedstock/process qualification route.
Initial samples: inspect dimensional and visual results, verify the agreed material condition, and check the intended assembly or moving function.
After any post-treatment: recheck critical dimensions, hardness or case requirements and surfaces that determine fit or wear.
Production release: agree on acceptance limits, sample/lot traceability, measurement frequency and changes that require requalification.
Examples of final-part checks: A case-hardened lever needs contact-condition and fit inspection after treatment. A gear assembly with Fe2Ni cage and plate needs material identification by component, followed by fit and movement testing. The published examples do not replace the actual project's dimensional or service-life qualification.
Illustrative inspection setup. It does not represent a certified inspection report or a confirmed Fe-2Ni production lot.
Production approval: Retain Fe-2Ni when both material properties and finished-part tests pass. Where evidence is incomplete, specify further trials; where the required condition cannot be achieved reliably or economically, compare another grade before volume production.
Provide the 2D drawing, 3D model, material callout, final hardness or strength requirements, critical tolerances and forecast volume. XTMIM can review Fe-2Ni material suitability, MIM geometry, tooling risks and the proposed sample-inspection plan. Any unqualified material or treatment requirements must be tested before production performance is agreed.